Follow us:-

API5L X56 PSL2 LSAW steel pipeline

  • 163 Views
  • 11-May-2024

API5L X56 PSL2 LSAW steel pipeline has a range of yield strength of 386-544 Mpa.API5L X56 PSL2 LSAW steel pipeline chemical composition,0.24 max for carbon,1.40 max for Mn,0.025 max for P,0.015 max for S,0.04 max for Ti. It can be applied as construction pipes on offshore platform, power station, petrochemistry and city construction etc.

API5L X56 PSL2 LSAW pipeline Chemical composition (Max)

Grade

C

Mn

P

S

Ti

X56

0.24

1.40

0.025

0.015

0.04

API5L X56 PSL2 LSAW steel pipe Mechanical properties (Min)

Grade

Yield Strength (Mpa)

Tensile Strength(Mpa)

X56

386-544

490-758

KUNFENG steel is a exporter & manufacturer of API5L X56 PSL2 LSAW steel pipeline for more than 10 years with reliable quality, competitive price and fast delivery.Please do not hesitate to contact me.if you have any queires on our API5L X56 PSL2 LSAW steel pipeline!Please do not hesitate to contact me.We will offer our warm-hearted service to you !

Related Post

ASTM 6150 Hot rolled steel round bar, ASTM 6150 Forged steel round bar

ASTM 6150 steel round bar under ASTM A29 standards and it is a fine grained, highly abrasion resistant carbon-chromium alloy steel. More informational about ASTM 6150 steel round bar, please see the following.

25Cr2Mo1V Hot rolled steel bar, 25Cr2Mo1V Forged steel bar

25Cr2Mo1V features for its high strength and toughness,We have almost 750 ton steel bar of 25Cr2Mo1V Hot rolled and Forged steel round bar in stock. Any need in 25Cr2Mo1V Hot rolled and Forged steel round bar, please contact us!

6061 Aluminum Bar

KUNFENG Steel offers a wide range of advanced and standard aluminum machining services for aluminum products. We specialize in customized machining services to

430 Stainless Steel Pipe

Chemical Composition